Stainless steel grade 314 can be heat treated by annealing the material at 1038-1149°C (1900-2100°F), and then quenching in water or rapidly air cooling. Grade 314 steel can be hardened only through cold working. To perform machinability of grade 314, coolant and high-speed turning tools are recommended.

After slowly heating the material to 871°C (1600°F), it should be thoroughly soaked, and then followed by quickly heating to 1093 -1232°C (2000-2250°F) , to perform forging, flanging, or working.

Chemical Composition

C

Mn

P

S

Si

Cr

Ni

≤0.25%

≤2.00%

≤0.045%

≤0.030%

1.50-3.00%

23.00-26.00%

19.00-22.00%

Mechanical Properties

Tensile strength

689 MPa

99900 psi

Yield strength

345 MPa

50000 psi

Modulus of elasticity

200 GPa

29000 ksi

Elongation at break (in 50 mm)

40%

40%

Hardness, Rockwell B

85

85

Applications

  • High-Temperature applications
  • Furnace parts
  • Furnace conveyor systems
  • Heat Exchangers

Material Summary

Stainless steel grade 314 has excellent high-temperature resistance characteristics among the chromium-nickel steels series. The silicon content in this material improves oxidation and carburization resistance; however, it can become very brittle when subjected to prolonged temperatures of 649-816°C (1200- 1500°F).

Manufacturing Process

Stainless steel grade 314 can be heat treated by annealing the material at 1038-1149°C (1900-2100°F), and then quenching in water or rapidly air cooling. Grade 314 steel can be hardened only through cold working. To perform machinability of grade 314, coolant and high-speed turning tools are recommended.

After slowly heating the material to 871°C (1600°F), it should be thoroughly soaked, and then followed by quickly heating to 1093 -1232°C (2000-2250°F) , to perform forging, flanging, or working.

If you have any enquiry about quotation or cooperation,please feel free to email us at or use the following enquiry form. Our sales will contact you within 24 hours. Thank you for your interest in our products.